INL materials scientist Subhashish Meher uses a local electron atom probe at the Center for Advanced Energy Studies to study the microstructure of treated superalloys.

Researchers at Idaho National Laboratory have discovered how to make "superalloys" even more super, extending useful life by thousands of hours. The discovery could improve materials performance for electrical generators and nuclear reactors.

The key is to heat and cool the superalloy in a specific way. That creates a microstructure within the material that can withstand high heat more than six times longer than an untreated counterpart.

"We came up with a way to make a superalloy that is much more resistant to heat-related failures. This could be useful in electricity generators and elsewhere," said Subhashish Meher, an INL materials scientist. He was lead author of a new Science Advances paper describing the research.

Alloys are combinations of two or more metallic elements. Superalloys are exceptionally strong and offer other significantly improved characteristics due to the addition of trace amounts of cobalt, ruthenium, rhenium or other elements to a base metal. Understanding how to build an improved superalloy is important for making the metallic mixture better for a particular purpose.

INL scientists have been studying nickel-based superalloys. Since these superalloys can withstand high heat and extreme mechanical forces, they are useful for electricity-generating turbines and high-temperature nuclear reactor components.

Previous research had shown that performance can be improved if the material structure of the superalloy repeats in some way from very small sizes to very large, like a box within a box within a box.

This is called a hierarchical microstructure. In a superalloy, it consists of a metallic matrix with precipitates, regions where the composition of the mixture differs from the rest of the metal. Embedded within the precipitates are still finer-scale particles that are the same composition as the matrix outside the precipitates - conceptually like nested boxes.

Meher and his coauthors studied how these precipitates formed within a superalloy. They also investigated how this structure stood up to heat and other treatments.

They found that with the right recipe of heating and cooling, they could make the precipitates two or more times larger than would be the case otherwise, thereby creating the desired microstructure.

These larger precipitates lasted longer when subjected to extreme heat. Moreover, computer simulation studies suggest that the superalloy can resist heat-induced failure for 20,000 hours, compared to about 3,000 hours normally.

One application could be electrical generators that last much longer because the superalloy that they are constructed of would be tougher. What's more, INL scientists may now be able to come up with a procedure that can be applied to other superalloys. So, it may be possible to adjust a superalloy's strength, heat tolerance or other properties to enhance its use in a particular application.

"We are now better able to dial in properties and improve material performance," Meher said.

Research paper


Related Links
Idaho National Laboratory
Space Technology News - Applications and Research


Thanks for being here;
We need your help. The Space Media Network continues to grow but revenues have never been harder to maintain.

With the rise of Ad Blockers, and Facebook - our traditional revenue sources via quality network advertising continues to decline. And unlike so many other news sites, we don't have a paywall - with those annoying usernames and passwords.

Our news coverage takes time and effort to publish 365 days a year.

If you find our news sites informative and useful then please consider becoming a regular supporter or for now make a one off contribution.
SpaceMediaNetwork Contributor
$5 Billed Once


credit card or paypal
SpaceMediaNetwork Monthly Supporter
$5 Billed Monthly


paypal only


TECH SPACE
Electronic skin points the way north
Dresden, Germany (SPX) Nov 16, 2018
While birds are able to naturally perceive the Earth's magnetic field and use it for orientation, humans have so far not come close to replicate this feat - at least, until now. Researchers at the Helmholtz-Zentrum Dresden-Rossendorf (HZDR) in Germany have developed an electronic skin (e-skin) with magnetosensitive capabilities, sensitive enough to detect and digitize body motion in the Earth's magnetic field. As this e-skin is extremely thin and malleable, it can easily be affixed to human skin t ... read more

Comment using your Disqus, Facebook, Google or Twitter login.



Share this article via these popular social media networks
del.icio.usdel.icio.us DiggDigg RedditReddit GoogleGoogle

TECH SPACE
EU court backs Dyson on vacuum cleaner energy tests

Mining bitcoin uses more energy than Denmark: study

Spain's Ibedrola sells hydro, gas-powered assets in U.K. for $929M

How will climate change stress the power grid

TECH SPACE
RUDN chemists made an electrode for hydrogen fuel production out of Chinese flour

Next-gen batteries possible with new engineering approach

Traditional eutectic alloy brings new hope for high energy density metal-O2 batteries

Pressure helps to make better Li-ion batteries

TECH SPACE
Roadmap to accelerate offshore wind industry in the United States

Denmark-based Orsted adds to its U.S. wind energy assets

Making wind farms more efficient

DNV GL successfully completed technical due diligence for 25 MW Windfloat Atlantic floating wind project

TECH SPACE
Solar panels for yeast cell biofactories

Freedom Solar Power launches first-of-its-kind commercial solar financing vehicle in Texas

Swiss company using concrete bricks to make renewables more stable, cheaper

New records in perovskite-silicon tandem solar cells through improved light management

TECH SPACE
Japan faces difficult energy choices

GE Hitachi and PRISM selected for US Dept of Energy's Versatile Test Reactor program

Global Nuclear Fuel's GENUSA Awarded Long-Term Fuel Supply Contract by TVO

Framatome marks opening of nuclear parts center at expanded solutions complex

TECH SPACE
Affordable catalyst for CO2 recycling

Bio jet fuels good for the climate, but technologies need tweaking

Cotton-based hybrid biofuel cell could power implantable medical devices

Wartsila, LUT University and Nebraska Public Power District to develop business case for alternative fuels

TECH SPACE
U.S. drivers to pay $80 million more this Thanksgiving

Crude oil prices test recent lows at start of holiday-shortened week

China's Xi in Brunei as oil-dependent sultanate seeks investment

Brunei to see Zhejiang Hengyi-built refinery operational by first half of 2019

TECH SPACE
Greenhouse gasses triggering more changes than we can handle

Online climate meet offers talkfest without the gas

Record-breaking Alps postcard sends message against climate change

Global warming has never stopped in the past hundred years









The content herein, unless otherwise known to be public domain, are Copyright 1995-2024 - Space Media Network. All websites are published in Australia and are solely subject to Australian law and governed by Fair Use principals for news reporting and research purposes. AFP, UPI and IANS news wire stories are copyright Agence France-Presse, United Press International and Indo-Asia News Service. ESA news reports are copyright European Space Agency. All NASA sourced material is public domain. Additional copyrights may apply in whole or part to other bona fide parties. All articles labeled "by Staff Writers" include reports supplied to Space Media Network by industry news wires, PR agencies, corporate press officers and the like. Such articles are individually curated and edited by Space Media Network staff on the basis of the report's information value to our industry and professional readership. Advertising does not imply endorsement, agreement or approval of any opinions, statements or information provided by Space Media Network on any Web page published or hosted by Space Media Network. General Data Protection Regulation (GDPR) Statement Our advertisers use various cookies and the like to deliver the best ad banner available at one time. All network advertising suppliers have GDPR policies (Legitimate Interest) that conform with EU regulations for data collection. By using our websites you consent to cookie based advertising. If you do not agree with this then you must stop using the websites from May 25, 2018. Privacy Statement. Additional information can be found here at About Us.